Polishing Imron?
#3
Registered
Join Date: Aug 2005
Location: Charlotte, NC
Posts: 147
Likes: 0
Received 0 Likes
on
0 Posts
![Default](/forums/images/icons/icon1.gif)
AMEN Ginger! We used Imron esclusively at FPB and after a few weeks, it is like Awlgrip! # 2000 W/D is about all you would want to sand with and then it will take 2 or 3 compounds and graduated pads to keep from "swirling up." When it gets outside, you will be able to see the buff marks unless you have a few years under your belt. Goob luck!