Paint stainless props to reduce galvanic corrosion?

Notices

Paint stainless props to reduce galvanic corrosion?

Thread Tools
 
Old 03-26-2008, 09:59 AM
  #1  
Gold Member
Gold Member
Thread Starter
 
Join Date: Oct 2006
Location: Newark, DE
Posts: 43
Likes: 0
Received 0 Likes on 0 Posts
Default Paint stainless props to reduce galvanic corrosion?

I'm curious. I've done a lot of research on galvanic corrosion and am wondering if one could paint their stainless props to reduce it. I've never seen or heard of it being done.
siearly is offline  
Old 03-26-2008, 10:41 AM
  #2  
Registered
 
Join Date: Apr 2005
Location: San Diego, Ca
Posts: 952
Likes: 0
Received 1 Like on 1 Post
Default

The paint won't stick around long enough. If the boat never left the dock the paint would slow the activity.
Westcoast is offline  
Old 03-26-2008, 08:07 PM
  #3  
Registered
 
Join Date: Nov 2003
Location: Antioch, IL
Posts: 817
Received 28 Likes on 19 Posts
Default

Agreed, any paint that would be efficient enough would gas and peel too fast.
RBeyer is offline  
Old 03-26-2008, 09:23 PM
  #4  
Registered
 
Join Date: Jul 2005
Location: evansville In
Posts: 482
Likes: 0
Received 0 Likes on 0 Posts
Default

Hey Siearly, Are you in fresh or salt water? If you are in fresh sometimes you need to go with Magnesium instead of alum. It is much softer and works really well!
speedreeder is offline  
Old 03-26-2008, 11:28 PM
  #5  
Registered
 
Join Date: Mar 2008
Posts: 206
Likes: 0
Received 0 Likes on 0 Posts
Default

Originally Posted by speedreeder
Hey Siearly, Are you in fresh or salt water? If you are in fresh sometimes you need to go with Magnesium instead of alum. It is much softer and works really well!
He means magnesium anodes (aka zincs) instead of aluminum. Also, you can get a prop zinc as well- this is required on Bravo 3 drives, and can be installed on Bravo 1 and 2 as well. Check out Boatzincs.com - its about $65 for a kit.
dogturd21 is offline  
Old 03-27-2008, 08:11 AM
  #6  
Registered
 
Join Date: Aug 2005
Location: Ray Twp. Michigan
Posts: 812
Likes: 0
Received 1 Like on 1 Post
Default

If you dont have them consider adding a merchathode system or make sure the one you have works.Also if you have shore power and use consider adding a galvanic isolator.
johnny b good is offline  
Old 03-27-2008, 12:39 PM
  #7  
Platinum Member
Platinum Member
 
26sonic's Avatar
 
Join Date: Feb 2001
Location: poughkeepsie, ny, usa
Posts: 1,198
Likes: 0
Received 0 Likes on 0 Posts
Default

so what zincs for brackish water alum. or mag. ?
26sonic is offline  
Old 03-27-2008, 04:25 PM
  #8  
Registered
 
Join Date: Mar 2008
Posts: 206
Likes: 0
Received 0 Likes on 0 Posts
Default

Brackish water should be aluminum. Only use magnesium in 100% fresh water.
dogturd21 is offline  
Old 03-28-2008, 06:17 AM
  #9  
VIP Member
VIP Member
 
Join Date: Feb 2001
Location: virginia
Posts: 548
Likes: 0
Received 1 Like on 1 Post
Default

Props are painted/ coated all the time - how many black aluminum props have you seen ? Paint is not smart enough to know the difference between Aluminum & stainless - Pre-treat the Ss prop with passivation or better yet with a blast profile of 1 - 1.5 mils in profile depth. Paint the props using epoxy. A Novalac epoxy or Cycloaliphatic Amine Epoxy will give you a good dense surface that will be most resistant to cavitation bubbles, however a simple polyamide epoxy will work well. With a blast prepared surface you can expect adhesion pull test numbers to be above 2,500 psi. Reducing the total amount of wetted SS surface will reduce the corrosion rate on exposed less noble metals. Even if you run the prop into a sand bar, not all the paint will come off and you will still have a lower corrosion rate of other metals because of the reduced exposed ss - Keep your dry film thickness low for best result - probably 3-4 mils. If you get lazy - an "epoxy powder coat" not polyester, will also work.
James is offline  
Old 03-28-2008, 11:14 PM
  #10  
Registered
 
Join Date: Sep 2007
Location: Tulsa, Ok
Posts: 166
Likes: 0
Received 0 Likes on 0 Posts
Default

Shazaaaaum!
Planetwarmer is offline  


Quick Reply: Paint stainless props to reduce galvanic corrosion?


Contact Us - Archive - Advertising - Cookie Policy - Privacy Statement - Terms of Service

Copyright © 2024 MH Sub I, LLC dba Internet Brands. All rights reserved. Use of this site indicates your consent to the Terms of Use.